Most rutile blue glazes on my clay at the temps I bisque to apply at a =
specific gravity of about 1.58. Your milage will almost certainly vary, =
depending on your bisque temp, clay, and how long you hold the pot in =
the glaze. This might be a starting point for tests.

Regards,
Jim