search  current discussion  categories  techniques - throwing 

slab throwing...... was clay decompressing......

updated tue 26 nov 02

 

Catherine White on mon 25 nov 02


I call it flinging. Same difference, though...... except I work on my
canvas covered board at waist level, and I throw the blob of clay away from
me at a shallow angle. Same as you, I rotate it 90º or 180º after each
fling. Fast and easy.

Best wishes,
Catherine in Yuma, AZ
My inability to emulate occasionally results in originality.
========================================
> > What do you mean by "tossing slabs?"
=========================================
> Take a good size lump of clay and throw it down on the bench (floor any
> firm surface, whatever) until it's a bit flat then start throwing it at
> an angle towards you. You'll see it start to flatten out and spread.
> Turn it 90 degrees each time you throw it.
>
> It doesn't take a lot of effort and if you do it fairly gently, the
> slabs will be of a more even thickness:
=============================