>strontium and whiting are completely different chemically

updated thu 28 nov 02

 

Ababi on wed 27 nov 02

specking.

Let me disagree with you!

-
>Strontium and Whiting are completely different chemically specking.

This glaze I use as clear part of my decorative combination

It used to be
SILICA 26.00
ENGLISH KAOLIN CC31 5.00
ZINC OXIDE 10.00
FELDSPAR SODA F7/SE 35.00
Calcium Carbonate 13.00
Barium 9.00
Bentonite 2.00

I made a high cost version

SILICA 26.00
ENGLISH KAOLIN CC31 5.00
ZINC OXIDE 10.00
FELDSPAR SODA F7/SE 35.00
Calcium Carbonate 13.00
strontium 7.00
Bentonite 2.00
And a lower cost for my students
KOREN GIR GIR in Hebrew= Whiting
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Cone 6
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

SILICA 26.00
ENGLISH KAOLIN CC31 5.00
ZINC OXIDE 10.00
FELDSPAR SODA F7/SE 35.00
Calcium Carbonate 22.00
Bentonite 2.00
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

If you see Kat, they are side by side in the table of elements.
In the case of this glaze the whiting is kind of make the color whiter ( on my buff
colored claybody).
The question is different , Randy, What is this glaze and what do you want it for. If it is
a turquoise glaze, I would think twice, though the calcium might be good too. If the
strontium in this glaze is just a flux, perhaps the creator of the glaze had it on hand?
You can replace it.
If you want you can e mail me the recipe.
To Kat ( with the hat that just now left the hut whom I don't hate): Numbers are good
but should not overrule as.
Ababi Sharon
Glaze addict
Kibbutz Shoval Israel