I've read the extensive amount of info. on this glaze in ^6 and understand
that the glaze can even be used at cone 10. I was wondering if anyone has
any suggestions for me when firing this glaze at ^10. I'm finding that its
a runner. The glaze formula that I have is as follows:

Lithium Carbonate 1.0
Strontium Carbonate 20.0
Neph Sy 60.0
(OM 4) Ball Clay 10.0
Flint 9.0


Titanium Dioxide 5.0
Copper Carbonate 5.0

Any advice would be greatly appreciated. Thanks, Jen

John Weber on sat 30 nov 02


Switch the Neph sy for a potash feldspar like G-200