Virgil and Susan Leise on tue 26 nov 02


Hi, Long ago at school I mixed up 3 experimental batches of salt =
bodies. I never did get to actually fire them in the salt kiln as the =
student that was doing that ...didn't get it done!!! Any how..I made =
notes that this body threw very well....and that is all I can tell you. =
The Pottery teacher gave this to me.

Salt Clay Body
XX Sagger 12
AP Green 6
Ball Clay 6
Custer 2