Elizabeth Fisher on tue 3 dec 02


Not a problem. Actually, I think I have successfully "fixed" the
problem. As cracks were hardly bigger than hairlines, I just mixed
acrylic paint to match, then brushed into cracks. It minimized them
enough, just by taking down the high contrast of black crack showing
in light colored piece, that I think I am ok. goal for next time
though is no more cracks=8A


Liz Fisher






>At 09:23 PM 12/2/02 -0500, you wrote:
>>>If the work doesn't stand on its own as a fine example of
>>>your work, don't show it. No excuses.
>
>>Whoa! I am with you. Points taken...
>
>
>Sorry; shouldn't have used your personal circumstance
>as an opportunity to wear my soapbox out! It was a
>topic that had some up recently with a student,
>though, and I was on a roll...nothing personal!
>
> -Snail
>
>___________________________________________________________________________=
___
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.