Hi Friends, can anybody give me any tips about using Classic Crackles CC102
White which comes in a pint jar from Mayco? My usual work is cone 6
stoneware with dip and pour glazes a la John/Ron, so this is a new one for me
as I see you fire it to cone 06. I understand about using India Ink or other
substances after firing to show up the crackle.....but if you have any
experience with this for decorative pieces please share? Thanks. Toni Smith
in Ohio