search  current discussion  categories  kilns & firing - coatings 

itc coating for industry

updated thu 12 dec 02

 

Leland G. Hall on tue 10 dec 02


Hi all. I know that some of you know Feriz Delcic (the developer of ITC
coatings?) personally. I posted this yesterday and got no response yet so
will try again. My brother is a lead millwright at a major metals plantand
has asked me for information on ITC. Teladyne is not likely to deal with a
small pottery supply. Or even a large one for that matter. Can someone
please guide me to a direct contact to International Technical Ceramics?
Internet searches are comeing up with pottery suppliers only.

Thank you
Leland Hall
Before The Wheel Enterprises
La Pine, Oregon

Nanci Bishof on tue 10 dec 02


Leland,

Feriz Delkic can be reached at the factory in Mayport, a section of
Jacksonville, FL.
His number at the factory is 904 285 0200. His ITC 100 is distributed
worldwide. Some of his customers are Teledyne Alvac, NASA & potters you know
and respect such as Mel. ITC is utilized in furnaces, lighting fixtures,
kilns and a host of other applications. He'll be happy to speak with you. I
let him know you will be contacting him.

nanci bishof

bob huskey on wed 11 dec 02


Leland, maybe this will be helpfull:


International Technical Ceramics Incorporated
POB 1726
Ponte Vedra, FL 32004
904-285-0200

I don't think that they have a web site. Bob Huskey--
Tallahassee,florida

----- Original Message -----
From: "Leland G. Hall"
To:
Sent: Tuesday, December 10, 2002 1:30 PM
Subject: ITC coating for industry


> Hi all. I know that some of you know Feriz Delcic (the developer of ITC
> coatings?) personally. I posted this yesterday and got no response yet so
> will try again. My brother is a lead millwright at a major metals
plantand
> has asked me for information on ITC. Teladyne is not likely to deal with
a
> small pottery supply. Or even a large one for that matter. Can someone
> please guide me to a direct contact to International Technical Ceramics?
> Internet searches are comeing up with pottery suppliers only.
>
> Thank you
> Leland Hall
> Before The Wheel Enterprises
> La Pine, Oregon
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
>