Vince said
of a softbrick stacked door is that the bricks tend to erode quickly =
from
stacking and unstacking.>

A good way to slow this erosion down is to dip the 5 cold faces of the =
soft door brick in a very thin mortar or Greenpatch to give them a =
tougher skin. I like the hot face coated with ITC.

Jim Larkin