search  current discussion  categories  glazes - traditional iron glazes 

carbon trap shino - your favorite glaze recipe?

updated tue 17 dec 02

 

clifton wood on mon 16 dec 02


a fellow student & i are exploring carbon trapping shinos this quarter... and
hopefully, beyond.

we started with the old issue of studio potter, and have since been reading up on
glazing & firing processes.

we're just bisquing our first 50 test cups / tumblers / vases... takes about 30 to
fill the gas kiln we'll be using.

and, of course, we've been gathering glaze recipes.

so -

if you have a favorite recipe for carbon trapping, we'd love to test it.

thanks in advance.

sabra
rochester ny