Leland G. Hall on wed 18 dec 02
Craig wrote: "They don't
contain Nepheline Syenite so I don't have to be concerned about long term
problems that arise from that stuff."
I have heard that Nepheline Syenite is somewhat soluble. But you use
problems, as in plural. I would like to know more please. Thanks.
Leland Hall
Before The Wheel Enterprises
La Pine OR, USA
Craig Martell on wed 18 dec 02
Leland asked:
>I have heard that Nepheline Syenite is somewhat soluble. But you use
>problems, as in plural. I would like to know more please.
Hello Leland:
Even though I used "problems", the only trouble I've had with Nepheline
Syenite is the deflocculating and settling of glazes from some soluble
Na. It's a very high sodium material and glaze fit is sometimes tricky but
it's really not too problematic in my experience.
regards, Craig Martell, Hopewell, Oregon
| |
|