Just one I haven't seen on the list, obviously not suited for the
production potter but it works for stuff like whistles, beads, little
figures, stuff I want to put in a pit fire: You can get food dehydrators
at garage sales pretty cheaply.... I usually have two going all summer
long but my old one has a rattle and an iffy thermostat, so I use it as
a pot dryer. light heat and circulating air....

Yours, kelly in ohio