How can I convert logicly frit 2120 to you materials without using solouble materials?
When I use frit 3110 I add borax, in this case I must remove something else.
Because I ask direcly frit to frit, I need your help

,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Cone deg.C. -
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

FRIT A 2120 p 100.0
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Seger Weight%
KNO 0.801 27.60%
CaO 0.199 6.20%
Al2O3 0.049 2.80%
SiO2 1.898 63.40%
Na2O 0.801 27.60%
Al:Si 38.39
Expan. 14.74
ST 254.94


,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Cone deg.C. -
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

FRIT 3110 100.0
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Seger Weight%
KNO 0.707 17.72%
CaO 0.293 6.34%
Al2O3 0.095 3.73%
B2O3 0.097 2.60%
SiO2 3.000 69.60%
K2O 0.064 2.32%
Na2O 0.643 15.40%
Al:Si 31.61
Expan. 10.95
ST 283.67
,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,

Ababi Sharon
Glaze addict
Kibbutz Shoval Israel
ababisha@shoval.org.il
http://members4.clubphoto.com/ababi306910/
http://www.milkywayceramics.com/cgallery/asharon.htm
and also
http://www.israel-ceramics.org/membersGallery/personalpage.asp?MID=507