Llewellyn Kouba on mon 30 dec 02
Some time ago I acquired a Basic Assortment of Kingpin Stilt Kit - numbers
2 Joe No1, 2 Joe No 2, 2 Joe No3, 2 Joe #4, 2 Joe NO 5-2, and 3 long bars
and 3 short bars. Can someone tell me what cone these might be rated to be
fired at? These were from Paragon Industries for an old Paragon
kiln. Thank you
Llewellyn Kouba
Arnold Howard on thu 2 jan 03
The Kingpin stilts were rated to 2000 deg. F. They were
manufactured at one time in Paragon's Mesquite, Texas plant.
Arnold Howard
Paragon
--- Llewellyn Kouba wrote:
> Some time ago I acquired a Basic Assortment of Kingpin Stilt Kit
> - numbers
> 2 Joe No1, 2 Joe No 2, 2 Joe No3, 2 Joe #4, 2 Joe NO 5-2, and 3
> long bars
> and 3 short bars. Can someone tell me what cone these might be
> rated to be
> fired at? These were from Paragon Industries for an old Paragon
> kiln. Thank you
>
> Llewellyn Kouba
__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com
| |
|