Gary C. Hatcher on sat 4 jan 03


I missed the discussion in December concerning bourry box kilns but for
those of you interested in bourry box kilns, I have posted about 50 new
photos of our kiln including packing, firing and construction at:
www.pinemills.com Click on red link at top of page.
It is a 128cu. ft. kiln
Fired to cone 12 in 18-24 hours, although could be fired in 8 but we have
extended the firings for ash effects.
Uses 2-3 cords of wood.

gary