search  current discussion  categories  kilns & firing - misc 

co2 and kilns

updated thu 30 jan 03

 

mel jacobson on wed 29 jan 03


thanks ron for that reminder about co2 in a
kiln room.

remember:
headache is the first line of defense when
firing a kiln.
if you get a headache, find out why...NOW.
it is probably carbon monoxide.

repeated headaches while firing is a sure
path to bad things.
mel
From:
Minnetonka, Minnesota, U.S.A.
web site: my.pclink.com/~melpots
or try: http://www.pclink.com/melpots