search  current discussion  categories  glazes - specific colors 

questions about the blues

updated mon 3 feb 03

 

Russel Fouts on sun 2 feb 03


Richard, Jeremy and Lily,

I have some questions about these blues.

The main question: Is there any special preparation for any of these?
(ball milling, grinding, aging 30 years, mixing only with neutral ph
purified spring water, etc?)

And specific questions:

Leach Chinese Cobalt (faux Gosu)
40 Manganese Ox.
30 Black Iron Ox
20 Black Cobalt Ox
10 Calcined Ochre (yellow? red?, ?)
100 Total

Jeremy Kaiser Blue (By Parts? Do you have Percentages?)
3 Cobalt Carbonate
2 Kaolin (EPK)
1 Manganese Dioxide
1 Red Iron Oxide (Normal, Spanish, Synthetic?)
7 Total

Cardew's Blue
20 Cobalt Carbonate
20 White Tin Ox
20 China Clay
15 Plastic Red Clay
10 Black Managnese Ox
10 Talc Schist
5 Fe2o3
100 Total

And the last question:
Jonny Lang started playing professionally when he was 12. What does a 12
year old know about the blues? ;-) (Sandy's gonna kill me)

Thanks in advance

Russel

--

Russel Fouts
Mes Potes & Mes Pots
Brussels, Belgium
Tel: +32 2 223 02 75
Mobile: +32 476 55 38 75

Http://www.mypots.com
Home of "The Potters Portal"
Over 1800 Pottery Links!
Updated frequently

"Is the Hokey Pokey really what it's all about?"