pugmill /s cracks

updated mon 10 feb 03

 

Polly Harris on sun 9 feb 03


If you will center the pug on its side - not the cut end - you will not have
any more problems with the s crack. The crack is the memory of the pugmill's
auger in the middle of the pug. I am a production potter that throws
thousands of pot a year with no cracks.

Polly the potter