search  current discussion  categories  forms - handles 

juice for perfect handles?

updated thu 20 feb 03

 

Megan Ratchford on wed 19 feb 03


Hi to everyone!!!
Last night one of the instructors at the college where I work =
brought in a water soluble polymer emulsion that he let us try for =
pulling handles. Seems it was all the rage in the 60's but has since =
disappeared. I would love to find out the brand name of a suitable =
substitute and to hear of any experience others may have had. The =
handles pulled like a dream and since they were done without water they =
were very stable. I would love to get my hands on some of this handle =
juice!!
Thanks!!
Megan Ratchford
In sunny Colorado wondering why the East Coast won't share it's snow =
with us (WINK)...