Craig Martell on thu 20 feb 03
Hello Clay Enthusiasts:
I'm making some porcelain body tests and can't find analyses for two clays
online. If any of you have these or a website where I could purloin an
analysis, I would be in your debt.
The clays are: ECC Standard Porcelain and Hywite Magnum.
thanx, Craig Martell Hopewell, Oregon
Ababi on fri 21 feb 03
The ECC are not so kind about analysis
Yet Tony Hansen is: http://www.digitalfire.com/material/m-0171b1.htm
for the standard Porcelain
Ababi
David Beumee on sun 23 feb 03
Chemical Composition for Standard Porcelain:
SiO2 48
Al2O3 36.5
TiO2 0.02
CaO 0.07
MgO 0.30
Na2O 0.10
L.O.I. 12.5
David Beumee
2/20/03 12:45:08 PM, Craig Martell wrote:
>Hello Clay Enthusiasts:
>
>I'm making some porcelain body tests and can't find analyses for two clays
>online. If any of you have these or a website where I could purloin an
>analysis, I would be in your debt.
>
>The clays are: ECC Standard Porcelain and Hywite Magnum.
>
>thanx, Craig Martell Hopewell, Oregon
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>
| |
|