Les Elford on fri 21 feb 03
I went to the arcives to look for Randy's Red what was the date for the recipe?
Your help would be appreciated.
Thanks from Les in the Rockys!
Add photos to your e-mail with MSN 8. Get 2 months FREE*.
Diane Winters on sat 22 feb 03
Hi Les,
After seeing your post I tried the same search, typing Randy's Red in =
the "For" window, and got nothing, just as you did. I then checkmarked =
with a click in the "Search substring" box, searched again, and got 104 =
hits. When it rains, it pours - you now can have a nice couple hours of =
reading and weeding out ahead of you. I'd start with the most recent =
and work back, as if anyone has reformulated the glaze for any good =
reason, you want the benefit of that input.
Have fun testing,
Diane Winters in Oakland/Berkeley where summer mysteriously prevails
Les wrote:
>I went to the arcives to look for Randy's Red what was the date for the =
>recipe?.com.=20
Mert & Holly Kilpatrick on sat 22 feb 03
The Randy's Red I have in my database is:
Flint 30
EPK 5
Kona F-4 20
Talc 13
Gerstley borate 32
Red iron oxide 15
Bentonite 2
My note says "Reposted to Clayart by Veena Raghavan 1/99."
Holly
----- Original Message -----=20
From: Les Elford=20
To: CLAYART@LSV.CERAMICS.ORG=20
Sent: Friday, February 21, 2003 10:15 PM
Subject: Help loking for Randy's Red wheree in the arcives?
I went to the arcives to look for Randy's Red what was the date for =
the recipe?
Your help would be appreciated.
Thanks from Les in the Rockys!
-------------------------------------------------------------------------=
-----
Add photos to your e-mail with MSN 8. Get 2 months FREE*. =
_________________________________________________________________________=
_____ Send postings to clayart@lsv.ceramics.org You may look at the =
archives for the list or change your subscription settings from =
http://www.ceramics.org/clayart/ Moderator of the list is Mel Jacobson =
who may be reached at melpots@pclink.com.
| |
|