search  current discussion  categories  glazes - cone 4-7 

^6 slip

updated mon 10 mar 03

 

Susan Fox-Hirschmann on thu 6 mar 03


I am looking for a resource for ^6 porcelain slip, somewhere on the east
coast or mid west.

Appreciate any info.

Thanks.
Susan
Annandale, VA

Lois Ruben Aronow on thu 6 mar 03


On Thu, 6 Mar 2003 08:31:34 EST, you wrote:

>I am looking for a resource for ^6 porcelain slip, somewhere on the east
>coast or mid west.
>
Most ceramic supply companies have it. Try Ceramic Supply of NY/NJ
(1-800-7CERAMICS) or Kickwheel Pottery Supply in GA. Don't know their
#, but they are at www.kickwheel.com. I'm sure Axner has some too
- www.axner.com.
--------------------------------------------
=46ine Craft Porcelain - New and Updated for 2003!!
http://www.loisaronow.com=20

Dai Scott on thu 6 mar 03


Susan, would that be for slip-casting or slip trailing? We have an easy
recipe for slip-casting that is just dry porcelain, water and Darvan.
Dai in Armstrong, BC

rob on fri 7 mar 03


Campbell's Ceramics makes a nice Cone 6 porcelain slip. Can I ship you
some?

Rob Van Rens
-at Pine Ridge Pottery Supply in Alexandria, VA


----- Original Message -----
From: "Lois Ruben Aronow"
To:
Sent: Thursday, March 06, 2003 5:04 PM
Subject: Re: ^6 slip


On Thu, 6 Mar 2003 08:31:34 EST, you wrote:

>I am looking for a resource for ^6 porcelain slip, somewhere on the east
>coast or mid west.
>
Most ceramic supply companies have it. Try Ceramic Supply of NY/NJ
(1-800-7CERAMICS) or Kickwheel Pottery Supply in GA. Don't know their
#, but they are at www.kickwheel.com. I'm sure Axner has some too
- www.axner.com.
--------------------------------------------
Fine Craft Porcelain - New and Updated for 2003!!
http://www.loisaronow.com

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Susan Fox-Hirschmann on sun 9 mar 03


Is it already defluccuated?? And where can I see the fired color?
CAn you send me a sample of the color it fires.
Thanks
Susan Fox Hirschmann
4810 Tabard Place
Annandale, VA 22003-4053

Also is Campbell mixing this slip, or some other company?