search  current discussion  categories  glazes - cone 4-7 

feb 03 ^6 tests

updated fri 7 mar 03

 

Martin A. Arkowitz on thu 6 mar 03


i checked john anthony's website and it was great to see all those glaze tests
results. but as i don't have val cushings's book could he post the glae formulas
for DK11 white satin liner, VC72, VC71 and VC 62. with that info in hand, some
of us might want to try these glazes and compare results with his pictures.

eleanor arkowitz,

hanover n.h. where it is a balmy 21 degrees-maybe we are over the sub-zero
days???