Charles wrote:
>You recently posted a list of Ravenscrag glazes at ^6. I copied out =
>three of them:
>Kat's Matte
>Glossy Base
>High Magnesium Matte
>Unfortunately, I lost the rest of the glazes. Could you post them =
>again?

Charles:

Check out the Ravenscrag web site at:

www.ravenscrag.com

The recipes posted there are accompanied with photos of the tests, and I have
posted more under the forum list. There is a glaze that is quite
similar to a floating blue as well. What I have found with Ravenscrag
glazes is that they are quite simple to layer, and I get the most interesting
effect by doing so. I am currently working on several tests for cone 10r.

I will continue to up-date the site, and post new info in the forum.
Charles if the recipes that you were looking for are not on the site
I will get them to you.

Take care
Kat in the Hat
kat@digitalfire.com