jeremy Kaiser on thu 6 mar 03
Everyone on here, my blue an white pieces came out wonderful. Each one is nice and blue. Richard, my blue can become a transparent wash. Second i get a digital camera, will send out pictures on the list.
My recipe goes like this for 20 grams of liquid
10 grams cobalt carbonate
4 grams red iron oxide
4 grams manganese dioxide
2 grams kaolin
mix with green tea that has been allowed to sit until consistency of thin syrup, more or less green tea for washes or specific lines. this mixture makes for very nice blues and a variety just depending on how many layers you put on in the same area.
---------------------------------