fw: david's black celadon

updated sat 22 mar 03

 

Rikki Gill on fri 21 mar 03


Sorry, I forgot to say that this is a cone 10-11 reduction glaze.


----- Original Message -----
From: "Rikki Gill"
To: "clayart"
Sent: Friday, March 21, 2003 10:30 AM
Subject: David's Black Celadon


> David's Black Celadon
>
> Custer 45.3 %
>
> Whiting 17.1
>
> Zinc Oxide 2.2
>
> EPK 10.6
>
> Flint [silica] 22.8
>
> + 8 % Black Iron Oxide.
>
> The original formular called for Red Iron Oxide, and
> 1/4 % bentonite, which I deleted.
>
> This is a very beautiful and reliable glaze. Never runs, but will
blister
> if too thick.
>
>
>