search  current discussion  categories  people 

hamada matte glz

updated mon 24 mar 03

 

Susan Beyer on sat 22 mar 03


anyone know of and would like to share,,,hamada matte glaze recipe.
used it here in central minnesota a few years back.
checked all my reference material and seem to have lost it!
cone 10 reduction.
thanks!
susan

Chris Stanley on sat 22 mar 03


http://www.utpb.edu/courses/arts4365/formulae/glaze/hamada.htm

I am looking for more Hamada recipes! If you have any, please send them
along!

Thanks
Chris

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG]On Behalf Of Susan Beyer
Sent: Saturday, March 22, 2003 9:32 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: hamada matte glz

anyone know of and would like to share,,,hamada matte glaze recipe.
used it here in central minnesota a few years back.
checked all my reference material and seem to have lost it!
cone 10 reduction.
thanks!
susan

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Donald G. Goldsobel on sat 22 mar 03


I had this in my files along with several other Hamada glazes. I have not
tried it and take no responisbility blah blah blah



Good luck

Donald Goldsobel in the sunny San Fernando Valley where we are having "
Chamber of Commerce" weather. Be right back have to unload a bisque







Hamada Matt Glaze



Barium


1.4%

Whiting
12.3%

Potash Feldspar
72.1%

Ball Clay
11.2%


100%

Zinc
11.1%

Copper Carbonate
.01%

Red Iron Oxide
3.5%

Rutile
2.8%


----- Original Message -----
From: "Susan Beyer"
To:
Sent: Saturday, March 22, 2003 7:32 AM
Subject: hamada matte glz


> anyone know of and would like to share,,,hamada matte glaze recipe.
> used it here in central minnesota a few years back.
> checked all my reference material and seem to have lost it!
> cone 10 reduction.
> thanks!
> susan
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Susan Beyer on sat 22 mar 03


gee thanks for all the info!

NOW i can stop tearing the studio apart looking for that lost scrap of paper
and get down to business!
should have thouhgt of this sooner...
susan

June Perry on sun 23 mar 03


Donald, can you recheck the hamada glaze our posted. It seems to only add up
to 97 instead of the 100 you posted.

Thanks
June Perry
http://www.angelfire.com/art2/shambhalapottery

Donald G. Goldsobel on sun 23 mar 03


June,

I never modified the glaze recipe. It came from a web site the origin of
which I do not recall. Some one will try it and let us know the outcome.
Right now I have no time to mix a batch. I must glaze a set of plates for a
dinner party next Sat.

Donald


----- Original Message -----
From: "June Perry"
To:
Sent: Sunday, March 23, 2003 4:55 AM
Subject: hamada matte glz


> Donald, can you recheck the hamada glaze our posted. It seems to only add
up
> to 97 instead of the 100 you posted.
>
> Thanks
> June Perry
> http://www.angelfire.com/art2/shambhalapottery
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.