iandol on wed 26 mar 03
Dear James Bowen,
To get a good appreciation of what Celadon Glazes are all about my =
suggestion is that you do as a did, go to your local library and order =
Celadon Blues by R. Tichane via Interlibrary Loan. Get the second =
edition if you can because it has some very good colour illustrations.
For a glaze claimed to be good sky blue celadon see page 76 in the CM =
for January. Unfortunately and uncharacteristically for CM the recipe is =
not given.
Hope that helps.
Best regards,
Ivor Lewis
| |
|