search  current discussion  categories  glazes - specific colors 

question about opal blue-gretchen

updated sun 30 mar 03

 

Gretchen Woodman on sat 29 mar 03


--- Chris Schafale wrote:
> I've posted the latest batch of mugs from the
> stay-at-home
> exchange in Room 4:
>
> www.lightonecandle.com/mugexframe.html
>
> Chris
>
>
> --
> Light One Candle Pottery
> Fuquay-Varina, North Carolina, USA
> (south of Raleigh, NC)
> www.lightonecandle.com
> candle@intrex.net
>
>
______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change
> your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be
> reached at melpots@pclink.com.


__________________________________________________
Do you Yahoo!?
Yahoo! Platinum - Watch CBS' NCAA March Madness, live on your desktop!
http://platinum.yahoo.com

Gretchen Woodman on sat 29 mar 03


Chris,

I have tried the Cindy Strand Opal Blue on some
pieces and I really like the color and fit. I wanted
to ask you if there have been any stability tests done
on it because I would like to make some flasks with
this glaze. Hope everything is going well for you-I
saw you in the Pottery magazine-Congratulations!
Thanks for your help!

Gretchen


---