highwater brownstone & blisters

updated mon 31 mar 03

 

Charles Moore on sun 30 mar 03


Chris,

I am not experiencing the blistering that you are reporting, and I am using
the glaze that you included below:

> The glaze, by the way, is the very simple 3134 50%, silica 25%,
> epk 25%, and variations thereof. Most of the variations have some
> cobalt, some iron, at least 4% rutile.

> Chris

In fact, I got the recipe from you. I use it on IMCO 1-C and Laguna Half
and Half, both fired to ^6.

Perhaps it is the clay that you are using.

Charles Moore