Hannah Brehmer on tue 22 apr 03
Many, many thanks to Ron Roy for his usual thoughtful and extensive =
comments about glaze stability. I do have your wonderful book, Ron, =
and I use it with my classes who fire at Cone 6 in electric kilns. =
As you said, at Cone 10 the glaze is likely to be more stable. =
Thanks also to Edouard Bastarache for taking the time to send his usual =
very complete review of lithium. I was glad to see that he found no =
problems connected to glazes and lithium leaching. I guess I'll give =
Cat Jarosz the final word......she said she has been using and enjoying =
her spodumene-glazed dinnerware since the 80's and she is still as crazy =
as ever. Love ya, Cat.
My best to all-
Hannah at Tahoe