Dear Terry Sullivan,=20

I recall doing firings where we placed our pots in saggars and filled =
them with charcoal, other carbonaceous materials and/or metallic salts =
back in 1982 at Pt Pirie TAFE under the direction of John Coulter. I =
wrote an article about this for the Art teachers which was published by =
the Arts Consultants in their quarterly newsletter.

Perhaps you could put your experience on the Time Line so that we can =
understand the historic perspective.

Best regards,

Ivor Lewis.