I am very glad that clayarters help me find the faults. I count on you for
that. Great help.

So far,
there is not result for Edwards November version, because I did not make the
test.
I could see the Chrome could not be properly measured so I dropped it.

Secondly, the Raspberry Purple, is actually Raspberry Blue. A nice blue.
I dropped the original chrome and tin and added only the RIO and Cobalt.
To get the purple, all 4 colorants are needed. Next batch. Another error,
another discovery.
A nice blue. So, there, Mel. Blue, blue, blue, blue. I have had such a