search  current discussion  categories  technology - internet 

your glaze test web site link?

updated sun 4 may 03

 

Marianne Lombardo on thu 1 may 03


Alisa,

Can you please post the link again to where you are showing photos of your
glaze tests? I'm looking forward to seeing them. And a big thank-you for
posting your test results.

Marianne

Donald Burroughs on sat 3 may 03


Hi Alisa
I would also like to have the link where you have posted visuals of glaze
tests. I have been following your test results for some time and would look
forward to any visuals you might have. I wolud also like to know if you can
share with us on this side of the Atlantic the equivalent frit formulas you
use when replacing a Ferro or other frit which is more common here.

Sincerely, Donald Burroughs
On the Web @ http://www.autobahn.mb.ca/~donaldo



On Thu, 1 May 2003 23:42:18 -0400, Marianne Lombardo
wrote:

>Alisa,
>
>Can you please post the link again to where you are showing photos of your
>glaze tests? I'm looking forward to seeing them. And a big thank-you for
>posting your test results.
>
>Marianne
>
>___________________________________________________________________________
___
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Alisa Clausen on sat 3 may 03


Dear Marianne,
The site will be ready for "public" eyes this week. I have the recent tests
posted, so those interested can get a view of them. It has been an exciting
and laborious project. Thanks to John Rodgers for working together with me
to get the photos posted on his site. I was so inspired that I bought a
domain and now have a site. Soon to be released! Thanks for asking
Marianne.

Regards from Alisa in Denmark