search  current discussion  categories  tools & equipment - slab rollers 

bailey slab roller....

updated thu 15 may 03

 

Sandy Miller on wed 14 may 03


I've had a DRD/II for about a month. Love it but after using a rolling =
pin for 18 years what can I say....
I'm not very mechanical and it came in several boxes. The only trouble =
I had in assembling was attaching the table top to the frame. The table =
top is supposed to be 1/8" from the roller (so the canvas doesn't get =
caught between the roller and top) They should put a shim in the =
package. Even when clamped down the top has a tendency to move. After =
uttering many blue smoke words I won't repeat, I cut my own shims. =
Worked great. I layed out my parts, read directions etc and still ended =
up putting it together and taking it apart several times. It really is =
great to use and beat a rolling pin hands down!
Sandy Miller=20
PS: my husband thought I did a great job, what a guy!