 try this one.  alkaline glaze cone 10 - 13         barium carbonate       36.6                         

                                                                                      lithium carbonate         1.1         

Josie Norman                                                          nepheline   syenite     45.6                                                                                                                                   

                            ball clay                             7.2

crackedpot933@earthlink.net                           flint  ( 200 mesh )               9.5  

Why Wait? Move to EarthLink.                           for carter add

                                                                                  silicon carbide                       1.0