search  current discussion  categories  kilns & firing - misc 

see the kiln/linda b's.

updated sat 24 may 03

 

mel jacobson on wed 21 may 03


i have a picture of the kiln built by linda, dannon, lori and bonnie.
go to my website, click below.
go to clayart page.
wait for it.. i left it a clear nice image...a bit large.
mel
From:
Minnetonka, Minnesota, U.S.A.
web site: my.pclink.com/~melpots
or try: http://www.pclink.com/melpots
new/ http://www.TICK-ATTACK.COM

Culling on fri 23 may 03


Congrats folks nice looking kiln - what is visible!!Where did the barrow
loads of castable go?
Steph


> i have a picture of the kiln built by linda, dannon, lori and bonnie.

Hendrix, Taylor J. on fri 23 may 03


I second Culling's comment. Handsome kiln surrounded by some handsome
women. Woohoo!

I think we need some more pictures of that nice kiln--some all around
shots.

Taylor, in Waco

-----Original Message-----
From: Culling [mailto:culling@KISSER.NET.AU]=20
Sent: Friday, May 23, 2003 12:14 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: see the kiln/linda b's.


Congrats folks nice looking kiln - what is visible!!Where did the barrow
loads of castable go?
Steph


> i have a picture of the kiln built by linda, dannon, lori and bonnie.

________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.