Kristin on mon 26 may 03
Jade greens and teal blue (not).
CT Red, Raspberry as Blue, Oil Spot.
Will the fun never end?
Two more glaze test pages added:
http://www.tamarac.net/kgspottery/glaze_tests.htm
Thanks all - Kristin
__________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
http://search.yahoo.com
Ababi on tue 27 may 03
Hello Kristin.
You better test on several claybodies for sure the Jade greens look better on a better
quality claybody. Much better buff mottled. In general the tests are looked very good I
suggest you to make some horizontal carves to se how the glaze acts when the
surface is changing.