Lily Krakowski on thu 5 jun 03
Aha! I knew the little aging GreyCells would click in sometime! They done
did!
Behrens. CERAMIC GLAZE MAKING. Copyright 1967, 11th Editon in 1998.
Under Wide-Range Firing Glazes. Several include Strontium! In an 02-5
glaze only 1.8% in an 04-4 one 13.7% and several have % of Strontium in
between those two points. Many of these glazes include Barium.... Someone
out there can try replacing ALL the Barium with Strontium and running with
it... (Where to I have no idea)
Lili Krakowski
P.O. Box #1
Constableville, N.Y.
(315) 942-5916/ 397-2389
Be of good courage....
| |
|