search  current discussion  categories  forms - misc 

exploding double walled bowls

updated sun 15 jun 03

 

Elca Branman on sat 14 jun 03


On Sat, 14 Jun 2003 11:28:14 EDT Susan Setley
writes:
He forgot to put an air escape hole in the lip and a large
> chunk of the lip
> blew out while bisquing. Fortunately it didn't damage anyone else's
> pots. He
> has a master's degree in fine arts/ceramics and he says that was the
> cause.

I knew advanced degrees were dangerous , but never realized that they
were potentially explosive...



Elca Branman

http://elcabranman.com

________________________________________________________________
The best thing to hit the internet in years - Juno SpeedBand!
Surf the web up to FIVE TIMES FASTER!