Dear John Rodgers,

Your mixture of Clay and Oak Ash has a lot of potential but the first =
thing you need to consider is the temperature at which your clay is =
expected to mature. This imposes limitations on the materials you can =
select to enable your basic material to fuse well to a glassy matrix =
which is well bonded to your clay.

Give me that information (Cone number and clay type) and I can give you =
positive, constructive, creative direction.