Arnold Howard on mon 30 jun 03


I suggest that you call Evenheat. They could quickly tell you about
those models:

989-856-2281

Sincerely,

Arnold Howard
Paragon Industries, L.P.
www.paragonweb.com



From: Karen Hein
> I have the option to purchase several Evenheat kilns that were left on
> a friends property. Both have what appears to be good firebrick &
have
> on/off switches and sitters which is fine. However, one has what
looks
> to be an orange coating on the firebrick (almost terra cotta like in
> color) and the other has what appears to be good firebrick, the
problem
> being it is NOT surrounded by insulation or stainless steel. the
> firebrick are held together by steel bands and the control panel is
attached
> to the brick.
>