artimator on mon 7 jul 03
Hi ya Josh,
Use draw rings to enable yourself to see whether or not you need =
more salt....I think we used to keep salting till the salt ran =
outHEHEHE......Several times we had white salt foam running out the =
cracks of the kiln onto the ground....what fun!!....Of course that is =
likely why we now have a soda kiln and our salt kiln is =
history.....Well, that, and the huge white cloud hovering over the =
parking lot...."Hey that is just fog!"HOHOHO....I love dat salt fire
PAX,
Rush
"I only indulge when I've seen a snake, so I keep a supply of =
indulgences and snakes handy"