search  current discussion  categories  kilns & firing - cones & controllers 

oxyprobe & thanks all for the tips of foamboard!

updated wed 16 jul 03

 

June Perry on tue 15 jul 03


Linda, my oxyprobe is doing the same thing. In the last firing I had to dig
up an old pyrometer to use because I couldn't get reading of temperature with
it. And like you, I had no trouble with the atmosphere readings.
I hope it's a simple fix or adjustment that we can do ourselves without
sending it "back to the shop". LOL
I had a problem with the atmosphere reading right after I got it and Nils
Lou fixed it pronto; but I did have to send it back. One of the little wires
had become loose or detached.

PS Thanks to all who wrote for tips on sources for the foam board!

Regards,
June
http://www.angelfire.com/art2/shambhalapottery