Earl,

Ian gave me a recipe to try for my "C" corner to get Tea Dust glazes for
c/5-11. It might be a good one for you to try. the recipe is:

50 K feldspar
20 Whiting
20 Dolomite
10 Spodumene
10 RIO

I haven't done it yet - let me know what your results are if you try it!