Val on thu 31 jul 03
Someone phonedme today to ask this question...she is doing heartboxes for a
wedding and she has been using a pink glaze..Mayco....after being fired thepieces
have been coming out with hard little bumps and the next group that was done
came out with the same on the lid but okay on the box part...and the glaze is all
streaky...does anyone have any idea?....old glaze....firing? poor greenware?...
ThanksBright Blessings
Val Mann, ww....