search  current discussion  categories  kilns & firing - raku 

copper and raku

updated sat 2 aug 03

 

Phyllis Tilton on fri 1 aug 03


Gene and Dolita: I think that I used the word 'sheet' when i should have used foil It is very thin. I am thinking that since you say it would be very runny, maybe the fish plaque could lay flat with the copper toward the middle. Seems I better use this raku firing to do some testing so that I would not ruin any other work. Thanks for responding.

Phyllis Tilton


---------------------------------
Do you Yahoo!?