search  current discussion  categories  glazes - faults 

glaze question: pinholing vases-suessed

updated fri 8 aug 03

 

Earl Brunner on wed 6 aug 03


Could you, would you with a fox? Could you, would you in a box?
I would not could not with a fox, I would not could not in a box. I do
no like green eggs and ham, I do not like them, Sam, I Am.

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Kathi
LeSueur
Sent: Wednesday, August 06, 2003 6:45 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Re: Glaze question: pinholing vases

mlkrakowski@CITLINK.NET wrote:

> Then:
> I have come up with yet another theory: that the glaze on the INSIDE
> of the
> belly is thicker than elswhere--not uncommon with closed shapes. that
the
> gasses it generates somehow are causing your troubles. Therefore fire
one
> vase unglazed on the inside.
>
> Could you? Would you?>>


Will do.

Kathi