I have mixed a batch of Turquoise glaze out of his Ceramic Glaze Handbook.
Cone 6 matt.

Anyone with experience with this glaze.
1. How thick to mix?
2. How thick to apply?

Randy
South Carolina

John Hesselberth on fri 22 aug 03


Hi Randy,

I can't answer your questions, but I would offer a caution. This glaze
is probably very unstable and I would bet it would fail the vinegar
test. It has a very low silica level (1.6). It should not be used on
functional work without thoroughly testing it.

Regards,

John
On Thursday, August 21, 2003, at 09:31 PM, ranmcc wrote:

> I have mixed a batch of Turquoise glaze out of his Ceramic Glaze
> Handbook.
> Cone 6 matt.
>
> Anyone with experience with this glaze.
> 1. How thick to mix?
> 2. How thick to apply?
>
> Randy
> South Carolina
>
> _______________________________________________________________________
> _______
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
>
http://www.frogpondpottery.com
http://www.masteringglazes.com