#6 tile clay

updated tue 26 aug 03

 

Norman van der Sluys on sun 24 aug 03


Has anyone had any experience using #6 tile clay or Saphire as a
substitute for EPK? The analysis I have seen shows a great similarity
to Epk, but are there issues about consistancy or particle size that
would make it a less reliable component?

Recent changes in my situation Have forced me to start from scratch
again, glazewise and I am on a very slim shoestring. The price
differential at my nearest large supplier is considerable. TIA

Norman van der Sluys
Benona Pottery
near the shore of Lake Michigan, where the muggy weather and
unpredictible showers announce the advent of Peach season, and the
lengthening hours of darkness harald the aproach of autumn.